Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® HIPS E

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Techmer ES
Trade Name Statiblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® HIPS E.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
ASTM D785
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
35.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 - 1.00e+11 ohm-cm
1.00e+8 - 1.00e+11 ohm-cm
ASTM D257
Surface Resistance 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
ASTM D257
Users viewing this material also viewed the following: