Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 65.0 °C @Thickness 0.749 mm |
149 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.17 mm |
149 °F @Thickness 0.125 in |
UL 746 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.00 mm |
149 °F @Thickness 0.0394 in |
ALL |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-G3 (Cond.) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G6 (Dry) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
UL746B |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.500 mm |
149 °F @Thickness 0.0197 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |