Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
Network Polymers NPP 50-0753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LB560401 High Density Polyethylene ApplicationsPetrothene LB560401 exhibits good stiffness and environmental stress crack resistance. Typical applications include household chemical and personal care product bottles.Regulatory Status.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
Ineos T50-800-01 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications Exact 0210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caul.. |
|||
Brittleness Temperature | -76.1 °C | -105 °F | ASTM D746 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Brittleness Temperature | -76.1 °C | -105 °F | ASTM D746 |
CPC - Vycom SEABOARD™ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil HDPE AS55-03 High Density Polyethylene Resin Product Description: AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a good balance of stiffness and stress crack resistance.Avail.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil HDPE BU46-060 High Density Polyethylene Resin Product Description: BU46-060 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin Product Description: BA50-120 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Compression molded; ASTM D746 |
Dow 620I Linear Low Density Polyethylene (LDPE) For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DMDA-8904 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested per ASTM D4976; ASTM D746 |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil HD 9856B Blow Molding Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ BA53-035 Blow Molding Resin
(discontinued **) BA53-035 is a high molecular weight, high density polyethylene copolymer offering an outstanding combination of stiffness and toughness. The resin provides superior melt strength and impact resista.. |
|||
Brittleness Temperature | -76.1 - -27.0 °C | -105 - -16.6 °F | Average value: -68.0 °C Grade Count:32 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **) AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **) AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack.. |