Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
Network Polymers NPP 50-1060 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
DuPont 20 Series 2020 Specialty Polyethylene Resin
(discontinued **) DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® ETP H4837 High Density Polyethylene ApplicationsALATHON H 4837 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color a.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Brittleness Temperature | -76.0 °C | -105 °F | ASTM D746 |
LyondellBasell Microthene® F FA70900 High Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Brittleness Temperature | -76.0 °C | -105 °F | ASTM D746 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LT570401 High Density Polyethylene ApplicationsPETROTHENE LT 5704-01 resin exhibits good stiffness and environment stress crack resistance. Typical applications are bleach and household chemical bottles.Regulatory StatusLT 5704-01 m.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<SUB>50</SUB>; ASTM D746 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Ultrathene® UE637000 Ethylene Vinyl Acetate Copolymer, Film Extrusion Grade ULTRATHENE UE637000 is an EVA copolymer with good toughness, flexibility and clarity. Applications include laminating and heavy duty films as well as injection and blow molding. UE637000 contains no.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® NA814000 Low Density Polyethylene ApplicationsPETROTHENE NA 814-000 is a low density homopolymer resin specifically developed for a wide variety of blow molding applications. This resin exhibits excellent gloss, an excellent balanc.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Teknor Apex TELCAR® 1050-75 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Borstar® ME6053 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar ME6053 is a natural, bimodal medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor made properties important in jacketing applications, .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis SuperTR™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables SuperTR LE4212 is a natural, crosslinkable low density polyethylene compound, which has water tree retardant and scorch retardant properties.SuperTR LE4212 has been specifically developed as a scorc.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
CPC - Vycom PLAYBOARD™ HDPE Sheet for Modular Playground Systems Playboard Modular Playground Systems consists of 2-color PolyCarve™ co-extruded sheet and Grip X™ slip resistant sheet materials.FEATURES AND BENEFITS Weather resistant- Playboard is UV stabilized.. |
|||
Brittleness Temperature | -76.1 °C | -105 °F | ASTM D746 |
ExxonMobil LL 5100.09 Compounding Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ AA45-004 Blow Molding Resin Product Description: AA45-004 is a blow molding high density polyethylene copolymer offering exceptional stress cracking resistance and impact performance.Availability: Latin America, North America .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8130 Polyolefin Elastomer Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process.. |
|||
Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE) Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme.. |
|||
Brittleness Temperature | -76.0 - -67.0 °C | -105 - -88.6 °F | Average value: -74.1 °C Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |