Material Notes:
Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent combination between thermal stability and mechanical properties. This grade is widely used for: Automotive parts-Cooling fan, Shaft gear; Electrical & electronic parts-Plug, housing; and Sport, industrial, construction parts-Joint bushing, Disc. This product is available in natural & black color and in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 0.80 %

@Temperature 23.0 °C,
Time 86400 sec
0.80 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D786
Tensile Strength, Yield 195 MPa
28300 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 270 MPa
39200 psi
ASTM D790
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 23.0 - 85.0 °C
2.50 µin/in-°F

@Temperature 73.4 - 185 °F
ASTM D696
Melting Point 262 °C
504 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.60 - 3.20 mm
HB

@Thickness 0.0630 - 0.126 in
ISO 1210
Oxygen Index 23 %
23 %
ISO 4589
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
flammability index; IEC-60695-2-12
650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
ignition temperature; IEC-60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 6.00e+13 ohm
6.00e+13 ohm
IEC 60093
Dielectric Constant 3.75
3.75
IEC60250
Dielectric Strength 40.0 kV/mm
1020 kV/in
IEC 60243
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 500 V
500 V
Solution B; IEC 60112
600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 270 - 275 °C
518 - 527 °F
Front Barrel Temperature 285 - 295 °C
545 - 563 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 275-285°C
Fire and smoke F index 2
NF F16 101, I2,F3
Users viewing this material also viewed the following: