Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 725 °C @Thickness 1.60 mm |
1340 °F @Thickness 0.0630 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 725 °C @Diameter 0.850 mm |
1340 °F @Diameter 0.0335 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Glow Wire Test | 725 °C @Thickness 0.800 mm |
1340 °F @Thickness 0.0315 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM Akulon® CO-KGV4 /A JN.00.86 PA6-GF20 FR % Glass Reinforced, Heat Stabilized, Flame Retardant (halogen-phosphorous-free) |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Glow Wire Test | 725 °C @Thickness 2.00 mm |
1340 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Glow Wire Test | 725 °C @Thickness 0.750 mm |
1340 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
Ignition Temperature; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Glow Wire Test | 725 °C @Thickness 0.900 mm |
1340 °F @Thickness 0.0354 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Glow Wire Test | 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |