Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 234 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ASTM D648
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6
15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics EXTEM UH1026 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear
LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66
LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for ..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66
LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66
LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66
LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C

@Thickness 3.20 mm
453 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ISO 75-1, 2
Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ISO 75-1, 2
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.