Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer Polyplastics Co.
Trade Name FR-PET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 134 MPa
19400 psi
ISO 527-1, 2
Elongation at Break 2.0 %
2.0 %
ISO 527-1, 2
Flexural Strength 203 MPa
29400 psi
ISO 178
Flexural Modulus 9.30 GPa
1350 ksi
ISO 178
Charpy Impact, Notched 0.860 J/cm²
4.09 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 234 °C
453 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
IEC 60093
Surface Resistance 3.00e+16 ohm
3.00e+16 ohm
IEC 60093
Dielectric Strength 23.0 kV/mm
584 kV/in
IEC 60243-1
Comparative Tracking Index 250 V
250 V
IEC 60112