Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6714.17 Injection Molding Resin
(discontinued **) HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
Lucent Polymers TPO-1015 Thermoplastic Polyolefin Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C @Thickness 3.20 mm |
100 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C @Thickness 3.20 mm |
100 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LLP8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil HD 6733.17 Injection Molding Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | |
Arkema Group Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 101 °C | 100 - 214 °F | Average value: 67.4 °C Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 °C | 100 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 38.0 - 55.0 °C | 100 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |