ExxonMobil LL 8555.25 Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil LL 8555.25 Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suited for applications that require the optimum balance of processability, stiffness and low temperature toughness. Availability: Latin America, North America and South America Additive: Stabilizer: YesMedium Term UV-4 Applications: Consumer ArticlesFine Threaded ContainersPlayground EquipmentPoint of Display CabinetsPotable Water TanksToys Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ESCR 100% Igepal® 300 hour
300 hour
ASTM D1693
ESCR 10% Igepal® 60 hour
60 hour
ASTM D1693
Melt Flow 6.8 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
6.8 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
1% secant; ASTM D790
Impact Test 81.3 J
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
60.0 ft-lb
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
ARM
217 J
<br>@Thickness 6.35 mm,<br> Temperature -40.0 °C
160 ft-lb
<br>@Thickness 0.250 in,<br> Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C
138 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648