Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 - 68.0 °C
147 - 154 °F
ASTM D648
Novatec Novacycle® 501 PVC
Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe..
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 68.0 °C
122 - 154 °F
Average value: 60.8 °C Grade Count:4
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..