Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0339T40L1 Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0339T40L1 Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
MD; ASTM D955
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM D638
Flexural Strength 47.0 MPa
6820 psi
ASTM D790
Flexural Modulus 4.200 GPa
609.1 ksi
ASTM D790
Izod Impact, Notched 0.251 J/cm
0.470 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C
183 °F
Users viewing this material also viewed the following: