Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60B Fluoroelastomer Compound Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B37, B38, EF31, EO78, F15, Z1. Z1 = compression set.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60D Fluoroelastomer Compound Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are re.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60E Fluoroelastomer Compound Litharge Incorporated, Green Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60H Fluoroelastomer Compound Fluoroelastomer Rubber, 60 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administra.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V70B Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V70W Fluoroelastomer Compound Off-white Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z1,.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V71H Fluoroelastomer Compound Green Fluoroelastomer Rubber, 70-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Ad.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V72G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperatures. Acc.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V75F Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 70-80 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V75G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 70-80 °IRHD. Diesel liner ring grade. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK707, A1-10, B38, EF31, EO78, F.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V75I Fluoroelastomer Compound Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1. Where Z1 = compressi.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V75M Fluoroelastomer Compound Brown Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1, Z2. Z1 = comp.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V75Y Fluoroelastomer Compound Yellow Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = co.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V76E Fluoroelastomer Compound ETP polymer. This peroxide cured compound is based on a tetrapolymer of Ethylene, Tetrafluoroethylene (TFE) and Perfluoromethylvinylether (PMVE), and a cure site monomer – 70-80 °IRHD.Applications.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V80D Fluoroelastomer Compound Fluoroelastomer Rubber, 75-84 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 80.Applications: Mouldings which are requ.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V80L Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B38, EF31, EO78, F15, Z1... |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V80Q Fluoroelastomer Compound Black Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administr.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V85F Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 80-90 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90D Fluoroelastomer Compound Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90E Fluoroelastomer Compound Special steam resistant, Green Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M3HK910, A1-10, B38, EF31, EO78, Z1.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M3HK914, A1-10, B38, EF31, EO78, Z1, Z2. Z1 = colour green, .. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90H Fluoroelastomer Compound Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administ.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90M Fluoroelastomer Compound Brown Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M3HK914, A1-10, B38, EF31, EO78, Z1, Z2, where Z1 = Brown and.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V90W Fluoroelastomer Compound Off-White Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admin.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V95F Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 85-95 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V95X Fluoroelastomer Compound Fluoroelastomer Rubber, 88 - 97 °IRHD. Copolymer of vinylindene fluoride and hexafluoropropylene. Gas-blister resistant fluoroelastomer rubber.Applications: Developed for oil field applications wh.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V97D Fluoroelastomer Compound Fluoroelastomer Rubber, 92-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. Tested at the Shell Thornton Research Centre, where it has shown excellent res.. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60K Fluoroelastomer Compound Fluoroelastomer Rubber, 55-65 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out: MHK610, A1-10, B37, B38, EF31, EO78. ASTM d.. |
|||
Flash Point | 315 °C | 599 °F | [°C] Auto-Ignition |
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Flash Point | >= 315 °C | >= 599 °F | |
Precision Polymer Engineering V60V Fluoroelastomer Compound Special steam resistant, Black Fluoroelastomer Rubber, 55-65 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out: MHK610, A1-10.. |