Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
ASTM E228-07 |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
CTE, linear | 13.3 µm/m-°C | 7.39 µin/in-°F | at Set Pt. |
Ferro EG 2783 Thick Film Glass Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 300 °C |
7.39 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8808 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCONEL® Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCONEL® Alloy HX A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high.. |