Polymer Property : CTE, linear = 52.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 94.0 µm/m-°C

@Temperature 0.000 - 800 °C
52.2 µin/in-°F

@Temperature 32.0 - 1470 °F
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti..
CTE, linear 94.0 - 130 µm/m-°C
52.2 - 72.2 µin/in-°F
Average value: 108 µm/m-°C Grade Count:6
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum..
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical LI-913 ASA, Injection Molding, High Impact
Information Provided by LG Chem
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
ASTM D696
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® EK1000 Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® EK1000-MP Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..
CTE, linear 94.0 µm/m-°C
52.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil..
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass F-Clean® Film for Greenhouses
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten..
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® ETFE
A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el..
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® ETFE Film
Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc.
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..