Polymer Property : CTE, linear = 53.9 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 75.0 - 97.0 µm/m-°C
41.7 - 53.9 µin/in-°F
Average value: 85.0 µm/m-°C Grade Count:7
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
CTE, linear 50.0 - 97.0 µm/m-°C
27.8 - 53.9 µin/in-°F
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
CTE, linear 28.0 - 97.0 µm/m-°C
15.6 - 53.9 µin/in-°F
Average value: 46.2 µm/m-°C Grade Count:35
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..