Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
CTE, linear | 75.0 - 150 µm/m-°C | 41.7 - 83.3 µin/in-°F | Average value: 108 µm/m-°C Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
LyondellBasell SEQUEL® 1480 Engineered Polyolefin Description: SEQUEL® 1480 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability,.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LI-941 ASA, Extrusion, High Heat Resistance Information Provided by LG Chem |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5404 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 5511 High Impact Polystyrene Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant Information Provided by LG Chem |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN133HR Heat Resistant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
CTE, linear | 75.0 - 110 µm/m-°C | 41.7 - 61.1 µin/in-°F | ASTM D696 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 100 °C |
41.7 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ CA1110/2AC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact.. |
|||
CTE, linear | 75.0 - 85.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 - 47.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific) Pa6 based unfilled GTX |
|||
CTE, linear | 75.0 - 85.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 - 47.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Noryl GTX GTX6013 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 526M02 High Tg Fiber Optic Adhesive TRA-BOND 526M02 is a two-part, low viscosity epoxy system that was developed specifically for fiber optic applications. This material is recommended for bonding fiber optic bundles, potting glass fi.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | ASTM D696 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 200H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 240W Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X0718 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® X0722 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | GB1036 |
Beijing Evergrow Resources Oilon Information provided by Beijing Evergrow Resources. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 20.0 °C |
41.7 µin/in-°F @Temperature 68.0 °F |
|
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
CTE, linear | 75.0 µm/m-°C | 41.7 µin/in-°F | GB1036 |
Beijing Evergrow Resources MC Nylon Information provided by Beijing Evergrow Resources. |
|||
CTE, linear | 75.0 µm/m-°C @Temperature 40.0 - 130 °C |
41.7 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |