CTE, linear 72.0 - 79.2 µm/m-°C
40.0 - 44.0 µin/in-°F
ASTM D696
Quantum Nylon 6/6
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 72.0 - 79.2 µm/m-°C
40.0 - 44.0 µin/in-°F
ASTM D696
Quantum Nylon 6/6 MoS2 Filled
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 10.0 - 79.2 µm/m-°C
5.56 - 44.0 µin/in-°F
Average value: 54.9 µm/m-°C Grade Count:23
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
CTE, linear 12.0 - 79.2 µm/m-°C
6.67 - 44.0 µin/in-°F
Average value: 28.1 µm/m-°C Grade Count:23
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
CTE, linear 18.0 - 79.2 µm/m-°C
10.0 - 44.0 µin/in-°F
Average value: 33.0 µm/m-°C Grade Count:7
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..