CTE, linear 9.00 - 12.0 µm/m-°C

@Temperature -40.0 - 125 °C
5.00 - 6.67 µin/in-°F

@Temperature -40.0 - 257 °F
IPC-TM-650.2.4.41
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform..
CTE, linear 10.0 - 12.0 µm/m-°C

@Temperature -40.0 - 125 °C
5.56 - 6.67 µin/in-°F

@Temperature -40.0 - 257 °F
IPC-TM-650.2.4.41
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o..
CTE, linear 4.00 - 12.0 µm/m-°C
2.22 - 6.67 µin/in-°F
MarkeTech Gadolinium silicate:Cerium (GSO:Ce; Gd2SiO5) Scintillator Crystal
Gadolinium silicate doped with cerium is a "fast" crystal and can be used as a protection scintillator. Its possible applications include computer tomography, spatial resolution of less than 1 mm. I..
CTE, linear 10.0 - 12.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 6.67 µin/in-°F

@Temperature 68.0 °F
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
CTE, linear 10.0 - 12.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 6.67 µin/in-°F

@Temperature 68.0 °F
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
CTE, linear 11.0 - 12.0 µm/m-°C

@Temperature 1000 °C
6.11 - 6.67 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-198 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).