Polymer Property : CTE, linear = 9.00 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 14.4 - 16.2 µm/m-°C
8.00 - 9.00 µin/in-°F
Average value: 15.5 µm/m-°C Grade Count:3
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
CTE, linear 14.4 - 16.2 µm/m-°C
8.00 - 9.00 µin/in-°F
Average value: 14.8 µm/m-°C Grade Count:4
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..