Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.200 - 0.400 W/m-K | 1.39 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Thermal Conductivity | 0.200 - 0.400 W/m-K | 1.39 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Thermal Conductivity | 0.300 - 0.401 W/m-K | 2.08 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Thermal Conductivity | 0.320 - 0.400 W/m-K | 2.22 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.357 W/m-K Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Thermal Conductivity | 0.288 - 0.400 W/m-K | 2.00 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.336 W/m-K Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Thermal Conductivity | 0.370 - 0.400 W/m-K @Temperature 100 - 100 °C |
2.57 - 2.78 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.385 W/m-K Grade Count:2 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Thermal Conductivity | 0.280 - 0.400 W/m-K | 1.94 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.360 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.300 - 0.401 W/m-K | 2.08 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Thermal Conductivity | 0.202 - 0.400 W/m-K | 1.40 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.249 W/m-K Grade Count:7 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |