Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.341 W/m-K Grade Count:15 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Thermal Conductivity | 0.340 - 0.440 W/m-K @Temperature 100 - 100 °C |
2.36 - 3.05 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.384 W/m-K Grade Count:15 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 237 PTFE, 25% Glass Fiber Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 252 PTFE, 28% Glass Fiber Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Thermal Conductivity | 0.340 W/m-K @Temperature 121 °C |
2.36 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |