Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.340 W/m-K @Temperature 121 °C |
2.36 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Pyrotek NAD-250 Structural Insulation Board NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guar.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM F433 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.341 W/m-K Grade Count:15 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Thermal Conductivity | 0.340 - 0.360 W/m-K | 2.36 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.344 W/m-K Grade Count:5 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Thermal Conductivity | 0.340 W/m-K @Temperature 100 °C |
2.36 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 237 PTFE, 25% Glass Fiber Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
Thermal Conductivity | 0.340 W/m-K @Temperature 121 °C |
2.36 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 53765 |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
Thermal Conductivity | 0.340 W/m-K | 2.36 BTU-in/hr-ft²-°F | For EVAL F101 |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |