Thermal Properties Metric English Comments
Thermal Conductivity 3.31 W/m-K

@Temperature 93.3 °C
23.0 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel Holder Block Steel, AISI 4150 Modified
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b..
Thermal Conductivity 3.31 - 3.46 W/m-K
23.0 - 24.0 BTU-in/hr-ft²-°F
Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive
Description: Master Bond Polymer System SUPREME 3AN is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and co..
Thermal Conductivity 3.31 - 3.46 W/m-K
23.0 - 24.0 BTU-in/hr-ft²-°F
Master Bond Supreme 3ANHT Epoxy Adhesives for Bonding Stainless Steel
Description: Master Bond Polymer System Supreme 3ANHT is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with good thermal conductivity and conve..