Polymer Property : Thermal Conductivity = 4.86 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.500 - 0.700 W/m-K
3.47 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Thermal Conductivity 0.600 - 0.700 W/m-K
4.16 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Thermal Conductivity 0.600 - 0.700 W/m-K
4.16 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Thermal Conductivity 0.600 - 0.700 W/m-K
4.16 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Thermal Conductivity 0.600 - 0.700 W/m-K
4.16 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Thermal Conductivity 0.0370 - 0.700 W/m-K
0.257 - 4.86 BTU-in/hr-ft²-°F
Average value: 0.378 W/m-K Grade Count:8
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Thermal Conductivity 0.500 - 0.700 W/m-K
3.47 - 4.86 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Thermal Conductivity 0.560 - 0.700 W/m-K
3.89 - 4.86 BTU-in/hr-ft²-°F
Average value: 0.617 W/m-K Grade Count:9
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Thermal Conductivity 0.300 - 0.700 W/m-K
2.08 - 4.86 BTU-in/hr-ft²-°F
Average value: 0.448 W/m-K Grade Count:14
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..