Polymer Property : Maximum Service Temperature, Air = 204.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon CP-594CX Bulk Compound
Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but ..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate
Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier
Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber..
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib..