Polymer Property : Thermal Conductivity = 0.510 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 W/m-K

@Temperature 427 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 801 °F
Pyrotek Dry Cathode Barrier Material
In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the ..
Thermal Conductivity 0.510 W/m-K

@Temperature 698 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Pyrotek Pyrocast AR LITE Castable Refractory
A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 130 Dense Refractory Castable
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 HS Dense Refractory Castable
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 1400 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable
Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by ..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Thermal Conductivity 0.510 - 0.610 W/m-K

@Temperature 600 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..
Thermal Conductivity 0.510 W/m-K

@Temperature 816 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..