Polymer Property : Thermal Conductivity = 0.770 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 W/m-K

@Temperature 205 °C
5.34 BTU-in/hr-ft²-°F

@Temperature 401 °F
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable
Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 C Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 Dense Refractory Castable
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 1300 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 1200 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..