Thermal Properties Metric English Comments
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 C Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 Dense Refractory Castable
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 1300 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 1200 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..