Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.770 W/m-K @Temperature 205 °C |
5.34 BTU-in/hr-ft²-°F @Temperature 401 °F |
|
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode.. |
|||
Thermal Conductivity | 0.770 - 0.870 W/m-K @Temperature 100 °C |
5.34 - 6.04 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.770 - 0.870 W/m-K @Temperature 100 °C |
5.34 - 6.04 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Thermal Conductivity | 0.770 - 0.870 W/m-K @Temperature 100 °C |
5.34 - 6.04 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |
|||
Thermal Conductivity | 0.770 - 0.870 W/m-K @Temperature 1300 °C |
5.34 - 6.04 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 160 H Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc.. |
|||
Thermal Conductivity | 0.770 - 0.870 W/m-K @Temperature 1200 °C |
5.34 - 6.04 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |