Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.38 - 1.48 W/m-K @Temperature 1300 °C |
9.58 - 10.3 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 170 Dense Refractory Castable Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v.. |
|||
Thermal Conductivity | 1.38 - 1.48 W/m-K @Temperature 1300 °C |
9.58 - 10.3 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 170 GM Dense Refractory Castable Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Thermal Conductivity | 1.29 - 1.49 W/m-K @Temperature 1400 °C |
8.95 - 10.3 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 1600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 185 T Dense Refractory Castable Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values .. |