Thermal Properties Metric English Comments
Solidus 138 °C
280 °F
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m..
Solidus 138 °C
280 °F
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 138 °C
280 °F
AIM 40Bi/60Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Solidus 138 °C
280 °F
AIM 54Sn/26Pb/20In Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Solidus 138 °C
280 °F
AIM 58Bi/42Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.