Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.56 g/cc
0.309 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 23

@Load 4.00 kg
23

@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 55.2 MPa
8010 psi
Elongation at Break 55 %
55 %
% elongation on 5.65 (sq. root Area) gauge length
Shear Strength 3.40 MPa
493 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
Heat of Fusion 44.8 J/g
19.3 BTU/lb
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C
0.0399 BTU/lb-°F
Solid
0.201 J/g-°C
0.0480 BTU/lb-°F
Liquid
Thermal Conductivity 19.0 W/m-K

@Temperature 85.0 °C
132 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 138 °C
280 °F
Eutectic
Solidus 138 °C
280 °F
Liquidus 138 °C
280 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 58 %
58 %
Tin, Sn 42 %
42 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000380 ohm-cm
0.0000380 ohm-cm