Material Notes:
Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.3 MPa
7000 psi
Shear Strength 52.0 MPa
7540 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C
0.0399 BTU/lb-°F
Solid
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 179 °C
354 °F
Eutectic
Solidus 179 °C
354 °F
Liquidus 179 °C
354 °F
Component Elements Properties Metric English Comments
Lead, Pb 36.1 %
36.1 %
Silver, Ag 1.4 %
1.4 %
Tin, Sn 62.5 %
62.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000145 ohm-cm
0.0000145 ohm-cm