Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
ASTM E 831 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 100 - 200 °C |
50.0 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 100 - 200 °C |
50.0 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
50.0 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Europe-Africa-Middle East) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent, OQ Quality |