Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East) Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
32.8 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
32.8 µin/in-°F @Temperature 32.0 - 194 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
32.8 µin/in-°F @Temperature 32.0 - 194 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 150 °C |
32.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific) LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 150 °C |
32.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 200 - 300 °C |
32.8 µin/in-°F @Temperature 392 - 572 °F |
DIN 53 752 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
32.8 µin/in-°F @Temperature 32.0 - 194 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
32.8 µin/in-°F @Temperature 32.0 - 194 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
32.8 µin/in-°F @Temperature 32.0 - 194 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |