Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 50.0 - 100 °C |
35.0 µin/in-°F @Temperature 122 - 212 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66 LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 50.0 - 100 °C |
35.0 µin/in-°F @Temperature 122 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 0.000 - 90.0 °C |
35.0 µin/in-°F @Temperature 32.0 - 194 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 150 °C |
35.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -40.0 - 150 °C |
35.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 150 °C |
35.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature 23.0 - 150 °C |
35.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |