SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
1.41 g/cc
0.0509 lb/in³
ISO 1183
Moisture Absorption 0.650 %
0.650 %
50% RH, 24 hrs; ASTM D570
1.14 %
1.14 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ASTM D955
0.0134 cm/cm

@Time 86400 sec
0.0134 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
ASTM D638
162 MPa
23500 psi
ISO 527
Elongation at Break 2.8 %
2.8 %
ASTM D638
3.0 %
3.0 %
ISO 527
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
10.68 GPa
1549 ksi
50 mm/min; ASTM D638
Flexural Strength 246 MPa
35700 psi
ASTM D790
255 MPa
37000 psi
ISO 178
Flexural Modulus 8.41 GPa
1220 ksi
ASTM D790
9.80 GPa
1420 ksi
ISO 178
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.65 J/cm
16.2 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 57.0 kJ/m²
27.1 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 J
6.64 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.43
0.43
ASTM D3702 Modified
Coefficient of Friction, Static 0.48
0.48
ASTM D3702 Modified
K (wear) Factor 320 x 10-8 mm³/N-M
159 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
31.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
63.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
249 °C

@Thickness 3.20 mm
480 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: