Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 10.0 - 177 °C | 50.0 - 350 °F | Average value: 73.0 °C Grade Count:3 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone Low viscosity, green coating for power resistors to 1100°F (593°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |