Polymer Property : Processing Temperature = 383 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 180 - 195 °C
356 - 383 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Processing Temperature 180 - 195 °C
356 - 383 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Processing Temperature 180 - 195 °C
356 - 383 °F
Mixture Zone
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film
The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu..
Processing Temperature 180 - 195 °C
356 - 383 °F
Mixture Zone
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film
Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil..
Processing Temperature 175 - 195 °C
347 - 383 °F
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 175 - 195 °C
347 - 383 °F
Taiwan Sheen Soon Sheenthane® A9070A Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 175 - 195 °C
347 - 383 °F
Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 175 - 195 °C
347 - 383 °F
Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 180 - 195 °C
356 - 383 °F
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 180 - 195 °C
356 - 383 °F
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 190 - 195 °C
374 - 383 °F
Injection
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer
Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 190 - 195 °C
374 - 383 °F
Injection
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer
Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 190 - 195 °C
374 - 383 °F
Injection
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer
Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 190 - 195 °C
374 - 383 °F
Injection
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 180 - 195 °C
356 - 383 °F
Plasticizing Zone
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..
Processing Temperature 180 - 195 °C
356 - 383 °F
Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU
Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.