Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 25.0 MPa
3630 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
100% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
300% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
Tear Strength 80.0 kN/m
456 pli
ASTM D624
Processing Properties Metric English Comments
Processing Temperature 175 - 195 °C
347 - 383 °F
Users viewing this material also viewed the following: