Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 400 - 420 °C | 752 - 788 °F | |
Victrex® HT™ P22 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo.. |
|||
Processing Temperature | 400 - 420 °C | 752 - 788 °F | |
Victrex® HT™ P22PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo.. |
|||
Processing Temperature | 400 - 420 °C | 752 - 788 °F | |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Processing Temperature | 410 - 420 °C | 770 - 788 °F | |
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK), High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCQ3025 Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 280 - 420 °C | 536 - 788 °F | |
Asahi Kasei ASACLEAN PX2 Purging Compound ASACLEAN PX2 Grade excels in purging super-engineering resins at processing temperatures of up to 420°C (790°F). PX2 Grade is the most powerful high temperature grade for cleaning hard-to-clean re.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCR3030F Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 400 - 420 °C | 752 - 788 °F | |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |