Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® HT™ P22PF Polyetherketone

Category Polymer , Thermoplastic , Polyketone
Manufacturer Victrex
Trade Name HT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® HT™ P22PF Polyetherketone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInformation provided by Victrex
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
ISO 1183
Density 1.30 g/cc
0.0470 lb/in³
Crystalline; ISO 1183
Particle Size 50 µm
50 µm
D<sub>50</sub>; ISO 13320-1
Viscosity 190000 cP

@Temperature 400 °C
190000 cP

@Temperature 752 °F
Melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 4.30 GPa
624 ksi
ISO 527
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 373 °C
703 °F
ISO 11357
Glass Transition Temp, Tg 152 °C
306 °F
Onset; ISO 11357
160 °C
320 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 400 - 420 °C
752 - 788 °F
Dry Time 3 hour

@Temperature 150 °C
3 hour

@Temperature 302 °F
5 hour

@Temperature 120 °C
5 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: