Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 30 - 35 min | 30 - 35 min | |
NextGen Adhesives P907-04 Fiber Optic Adhesive Description: NGAC P907-04 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | |
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | 100 gram batch |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Pot Life | 20 - 35 min | 20 - 35 min | 100 gram batch |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | 100 gram batch |
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper.. |
|||
Pot Life | 30 - 35 min @Temperature 24.0 °C |
30 - 35 min @Temperature 75.2 °F |
4 oz. mass |
BCC Products BC 6060 Epoxy Surface Coat/Casting BC 6060 is a blue epoxy, abrasion resistant surfacing resin. Commonly referred to as “die surface” material, this system may be applied by brush or if preferred, cast in thin sections to a maximum.. |
|||
Pot Life | 30 - 35 min | 30 - 35 min | |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |