Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 40 min | 40 min | |
Resin Technology Group 1114 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 222 A/B Filled Potting Compound
(discontinued **) Green dielectric structural casting adhesive for potting and embedding most colors. 100/30 variable ratio.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 227 A/B Filled Potting Compound
(discontinued **) Dielectric structural potting and embedding adhesive. White and most colors. 2/12 variable ratio.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 368 A/B Filled Potting Compound
(discontinued **) Mica-filled red potting, encapsulating, casting adhesive. 2/1 ratio.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 489 A/B Filled Potting Compound
(discontinued **) Gray and color versatile dielectric casing adhesive resurfacing epoxy. 100/50 variable ratio.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 78112 A/B Filled Potting Compound
(discontinued **) Machinable room temperature casting/tooling epoxy system. 100/8 ratio.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 7908-1A/5012B Filled Potting Compound
(discontinued **) Red dielectric abrasion resistant structural hard casting, potting, adhesive, resurfacing epoxy system. 100/5 ratio. Good heat sink; 61% filled.Information provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron 7908-2A/5012B Filled Potting Compound
(discontinued **) Green or colors dielectric heat sink 57% filled. 100/5.6 ratioInformation provided by Abatron. |
|||
Pot Life | >= 40 min | >= 40 min | |
Abatron AboCast 1 A/B Filled Potting Compound
(discontinued **) Standard colored seamless casting resin. 100/40 ratio.Information provided by Abatron. |
|||
Pot Life | 40 min | 40 min | |
Huntsman HY 265 Cycloaliphatic Amine Approx. H+ equivalent weight 94. Mix Ratio with GY 6010 is 50.Comments/Applications: Modified cycloaliphatic polyamine adduct. Excellent chemical resistance. Exceptional sulfuric acid (96-98%) r.. |
|||
Pot Life | 40 min | 40 min | |
Huntsman HY 847 Cycloaliphatic Amine Approx. H+ equivalent weight 75. Mix Ratio with GY 6010 is 40.Comments/Applications: Medium viscosity, high performance hardener for self-leveling flooring.Data provided by Ciba Specialty Chemical.. |
|||
Pot Life | 40 - 45 min | 40 - 45 min | |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Pot Life | 40 min | 40 min | |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Pot Life | 40 - 45 min | 40 - 45 min | |
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works. |
|||
Pot Life | 40 - 45 min | 40 - 45 min | |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Pot Life | 40 min | 40 min | |
Henkel Hysol EA 934NA Paste Adhesive System Two part adhesive system with superior strengthCures at room temperatureApplications: Potting Structural Repair Liquid Shim |
|||
Pot Life | 40 min | 40 min | |
Henkel Hysol EA 9359.3 Paste Adhesive System Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding |
|||
Pot Life | 40 min | 40 min | |
Henkel Hysol EA 9360 Paste Adhesive System Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim |
|||
Pot Life | 40 - 60 min | 40 - 60 min | 100 gram batch |
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
Pot Life | 40 - 50 min | 40 - 50 min | 100 gram batch |
Master Bond EP38CL Adhesive Features Toughness and Durability Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura.. |
|||
Pot Life | 40 min | 40 min | 25 grams |
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Pot Life | 40 min | 40 min | |
Tra-Con Tra-Bond 5126 Medium Viscosity Aerospace-Grade Epoxy Adhesive TRA-BOND 5126 AEROSPACE-GRADE EPOXY ADHESIVE is a two-part, clear (amber), medium viscosity, aerospace-grade epoxy adhesive system recommended for bonding a wide variety of materials for structural .. |
|||
Pot Life | 40 - 60 min | 40 - 60 min | 200 gram mass |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
Pot Life | 40 - 60 min | 40 - 60 min | 100 gram batch |
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at .. |
|||
Pot Life | 40 - 50 min | 40 - 50 min | 100 gram mass |
Master Bond Supreme 11AN Two Component, Heat Resistant Epoxy Adhesive Description: Master Bond Polymer Adhesive System Supreme 11AN is a two component thermally conductive heat resistant epoxy adhesive with a one-to-one mix ratio, by weight or volume. It readily devel.. |
|||
Pot Life | 40 min | 40 min | |
Loctite® Durabond® E-40FL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 40 min @Temperature 20.0 - 25.0 °C |
40 min @Temperature 68.0 - 77.0 °F |
|
Abatron AboCoat 8501-2/AboCure 8501-2 Clear Epoxy Coating AboCoat 8501-2 is a clear, light amber resin made of 85% solids. It has a viscosity of 21-23 poises and a weight of 9.3 lbs/gallon. AboCure 8501-2 is a clear, light amber converter made of 85% solid.. |
|||
Pot Life | 40 min @Temperature 25.0 °C |
40 min @Temperature 77.0 °F |
100 g |
Abatron AboCast 10-5/AboCure 50-12 Epoxy AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-12 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-12 is a clea.. |
|||
Pot Life | 40 min @Temperature 25.0 °C |
40 min @Temperature 77.0 °F |
200 g |
Abatron AboCast/AboCure 8110-2 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | 40 min | 40 min | 25 grams |
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st.. |