Processing Properties Metric English Comments
Feed Temperature 160 - 165 °C
320 - 329 °F
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut..
Feed Temperature 150 - 165 °C
302 - 329 °F
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film
The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar..
Feed Temperature 150 - 165 °C
302 - 329 °F
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..