Material Notes:
Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foam or foam-skin insulation. Applications: Borcell™ HE4873 is designed to use as physically foamed insulation for data cables. Borcell™ HE4873 meets the following material classification: ISO 1872-PE, KEGHN, 45-D045, and ASTM D1248 Type III, Class A, Category 3, Grade E1, E3. The following cable material standards are met by Borcell™ HE4873: EN 50290-2-23. Cables manufactured with Borcell™ HE4873 using sound extrusion practice normally comply with the following cable product standards: IEC 61156 and EN 50288.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ISO 1872-2/ISO 1183
Melt Flow 3.8 g/10 min

@Load 5.00 kg,
Temperature 140 °C
3.8 g/10 min

@Load 11.0 lb,
Temperature 284 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
1 second; ISO 868
Tensile Strength at Break 23.0 MPa
3340 psi
ISO 527
Elongation at Break 600 %
600 %
ISO 527
Thermal Properties Metric English Comments
Brittleness Temperature -76.0 °C
-105 °F
ASTM D746
Processing Properties Metric English Comments
Zone 1 160 °C
320 °F
Zone 2 170 °C
338 °F
Zone 3 215 °C
419 °F
Zone 4 205 °C
401 °F
Zone 5 210 °C
410 °F
Die Temperature 220 °C
428 °F
Head Temperature 220 °C
428 °F