RJ470MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate and is designed for high-speed injection molding and contains nucleating and demolding additives. Additivation has been optimized to provide good antistatic and demolding properties without blooming or plate-out problems. This polymer is a CR (controlled rheology) grade with narrow molecular weight distribution giving low warpage. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and impact strength at ambient temperatures. Applications: lids, square containers, and square boxes.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ISO 2039-2
Tensile Strength, Yield 30.0 MPa
4350 psi
50mm/min; ISO 527-2
Elongation at Yield 12 %
12 %
50mm/min; ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ISO 75-2
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high