Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 40.0 - 60.0 MPa | 5800 - 8700 psi | Post Pressure |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | Specific |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |
|||
Hold Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Xmod™ GB306SAF Polypropylene, Glass Fiber Reinforced Xmod™ GB306SAF is a 35 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. The product is available in standard black 9502. This mat.. |