Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Resin Technology Group 408 Oxy-Bond™ Electrically Conductive Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco.. |
|||
Cure Time | 3.00 min @Temperature 120 °C |
0.0500 hour @Temperature 248 °F |
|
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Cure Time | 3.00 min @Temperature 204 °C |
0.0500 hour @Temperature 399 °F |
|
Lord Adhesives Flocklok® 852 Flock Adhesive LORD Flocklok® 852 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res.. |
|||
Cure Time | 3.00 - 5.00 min @Temperature 150 °C |
0.0500 - 0.0833 hour @Temperature 302 °F |
|
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2020322D6 Platinum Polymeric Ink C2020322D6 is a screen printable Platinum ink designed for printing working electrodes in electrochemical sensor applications. The paste can be used to detect H2O2, is suitable for developing biose.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2061027P15 High Brightness Phosphor Ink (Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2100203D2 Silver Ink This product is part of a range of Heat Curable Inks. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has exce.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials D2070209P6 White Dielectric Paste This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 - 4.02 min @Temperature 121 °C |
0.0500 - 0.0670 hour @Temperature 250 °F |
|
Master Bond EP17HT-3 One component, snap-curing epoxy system Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p.. |
|||
Cure Time | 3.00 min @Temperature 95.0 °C |
0.0500 hour @Temperature 203 °F |
|
Tra-Con Tra-Bond 224-1 Rapid Room Temperature Cure Epoxy Adhesive TRA-BOND 224-1 room temperature curing epoxy adhesive develops structural strength rapidly. Unlike most "rapid cure" epoxies which gel in one or two minutes, TRA-BOND 224-1 adhesive exhibits a 30 mi.. |
|||
Cure Time | 3.00 min @Temperature 150 °C |
0.0500 hour @Temperature 302 °F |
|
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7.. |
|||
Cure Time | 3.00 min @Temperature 100 °C |
0.0500 hour @Temperature 212 °F |
|
Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning |
|||
Cure Time | 3.00 min @Temperature 232 °C |
0.0500 hour @Temperature 450 °F |
|
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu.. |
|||
Cure Time | 3.00 min @Temperature 232 °C |
0.0500 hour @Temperature 450 °F |
|
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var.. |
|||
Cure Time | 3.00 min @Temperature 246 °C |
0.0500 hour @Temperature 475 °F |
|
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade) 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate.. |
|||
Cure Time | 3.00 min @Temperature 140 °C |
0.0500 hour @Temperature 284 °F |
Dry to stack, at 50% humidity |
Blue River Coatings Semi-Transparent Wood Stain Concentrate BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent .. |
|||
Cure Time | 3.00 min @Temperature 155 °C |
0.0500 hour @Temperature 311 °F |
ts2 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 3.00 min @Temperature 130 °C |
0.0500 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2090210P12 Silver Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 3.00 - 4.98 min @Temperature 75.0 °C |
0.0500 - 0.0830 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Acrylic 4000 Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |